利用高钙粉煤灰生产粉煤灰水泥的试验研究
发布时间: 2006-04-02 00:00 查看: 5686次
张世贤 周 涛 王志全
研究了高钙粉煤灰水泥的细度及活性激发剂对其物理性能的影响。研究结果表明,高钙粉煤灰水泥的安定性和各龄期的抗折、抗压强度均随着水泥的细度的提高和活性激发剂的掺入而提高,活性激发剂具有加速水泥矿物和f-CaO水化的作用。采用525#熟料,掺加30%的高钙粉煤灰时,水泥的比表面积在340~400m2/kg和掺入1%的活性激发剂,能够稳定生产425#高钙粉煤灰水泥。
关键词: 高钙粉煤灰; 细度; 安定性; 激发剂
中图法分类号: TQ172.7
Experimental Research of Using High-Calcium Fly Ash Produ ced Fly Ash Cement
Zhang Shixian Zhou Tao Wang Zhiquan
Abstract: Studied the influence of the fineness of the ceme nt with high-calcium fly ash and active agent on the physical properties. The r esults showed that the flexible and compressive strengths at different ages and stability of the cement with high-calcium fly ash increased with the increasing of cement fineness and the adding of active agent, which accelerated the hydrat ion of the cement minerals and f-CaO. By using 525# clinker, in the case that adding 30% high-calcium fly ash and 1% active agent, 425# high-calcium fly ash cement with 340~400 m2/kg specific surface area can be stably produced .
Key words: high-calcium fly ash; fineness; stability; active agent
Zhang Shixian: Postgraduate, Postgraduate Department,WUT,W uhan 430070 ,China.
研究了高钙粉煤灰水泥的细度及活性激发剂对其物理性能的影响。研究结果表明,高钙粉煤灰水泥的安定性和各龄期的抗折、抗压强度均随着水泥的细度的提高和活性激发剂的掺入而提高,活性激发剂具有加速水泥矿物和f-CaO水化的作用。采用525#熟料,掺加30%的高钙粉煤灰时,水泥的比表面积在340~400m2/kg和掺入1%的活性激发剂,能够稳定生产425#高钙粉煤灰水泥。
关键词: 高钙粉煤灰; 细度; 安定性; 激发剂
中图法分类号: TQ172.7
Experimental Research of Using High-Calcium Fly Ash Produ ced Fly Ash Cement
Zhang Shixian Zhou Tao Wang Zhiquan
Abstract: Studied the influence of the fineness of the ceme nt with high-calcium fly ash and active agent on the physical properties. The r esults showed that the flexible and compressive strengths at different ages and stability of the cement with high-calcium fly ash increased with the increasing of cement fineness and the adding of active agent, which accelerated the hydrat ion of the cement minerals and f-CaO. By using 525# clinker, in the case that adding 30% high-calcium fly ash and 1% active agent, 425# high-calcium fly ash cement with 340~400 m2/kg specific surface area can be stably produced .
Key words: high-calcium fly ash; fineness; stability; active agent
Zhang Shixian: Postgraduate, Postgraduate Department,WUT,W uhan 430070 ,China.
>> 相关内容
- 低品质粉煤灰的活性激发研究 (点击:15743 次)
- 废石膏粉煤灰石灰结合料的研究 (点击:15675 次)
- 粉煤灰和矿渣影响混凝土碳化的因素及建议 (点击:17140 次)
- 粉煤灰、矿粉复合双掺在大体积混凝土配合比中的应用 (点击:21172 次)
- 劣质粉煤灰对混凝土性能的影响探讨 (点击:21863 次)
- 【技术交流】煤矸石材料填筑路基施工研究 (点击:15981 次)
- 粉煤灰水热合成沸石分子筛的研究进展 (点击:25037 次)
- 煤矸石特性与资源化利用研究分析,综合利用依然是大难... (点击:25036 次)
- 燃煤灰渣作为混凝土掺合料的新变化及其影响(原创) (点击:25409 次)
#
最新技术资讯
更多>>- IE expo China 2026第二十七届中国环博会 链接全球机遇 探索新兴动能
- 2026雅鲁藏布江水电站工程建设暨工程机械、建材机械、矿山机械、工程车辆及设备展览会...
- 近400家名企共秀环保 “黑科技”,2025广州环博会将于9月启幕
- 2025第三届河北智能矿山技术与装备展览会
- 2026世界煤炭科技创新大会暨世界煤炭工业博览会
- 【技术分享】以粉煤灰、赤泥、尾矿、气化渣、煤矸石等 工业固废为基本原料制备高性能...
- 【技术分享】助力“双碳”目标,响应低能耗绿色建筑趋势,一种粉煤灰及其它固体废渣复...
- 一种利用固体废渣制备人造砂子、石子、砂粉料的制备方法
- 粉煤灰“超细活化”成建筑新资源
- 关于粉煤灰循环利用的发明专利